Home Buy Now Tutorials Documentation Updates FAQ Feedback Contact
Buy Now Tutorials Documentation Updates FAQ Feedback Contact

Material thickness

In weld joints where the parent material has thin plate thickness it is advantageous for the fatigue strength. This can be accounted for with the thickness factor, picture 1. Normally the reference thickness should be the default value 15 mm.

Picture 1: Thickness factor

Picture 1: Thickness factor.

Picture 2: Thickness factor graphs

Picture 2: Thickness factor graphs.